Figure 1: Microscopic views of the fractured surfaces showing adhesive failure on post surface in G1 [A1: (×500), A2: (×2000)] and G4 [B1: (×80), B2: (×300)]and mixed failure in G4 [C1: (×20), C2: (×2000)]. Exposure of quartz fi bers (1) and presence of epoxy resins (2) between fi bers are observed